From mixed Bi₂O₃–WO₃ to single-phase Bi₂WO₆: phase evolution and gamma-ray shielding performance


KAYHAN M., KAYHAN E., ŞAHİN M. C.

Journal of the Australian Ceramic Society, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1007/s41779-026-01442-w
  • Dergi Adı: Journal of the Australian Ceramic Society
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus
  • Anahtar Kelimeler: Bismuth tungsten oxide, Solid-state synthesis, Radiation shielding materials, Gamma-ray attenuation, Monte Carlo simulation, Phy-X/PSD, Nuclear materials, Radiation protection
  • Uşak Üniversitesi Adresli: Evet

Özet

In this study, bismuth tungsten oxide powders were synthesized via a scalable solid-state reaction method at three different temperatures: 400 °C, 600 °C, and 800 °C. The effects of calcination temperature on structural, morphological and gamma-ray shielding properties were systematically investigated compared to the mixture sample of bismuth oxide and tungsten oxide. X-ray diffraction analysis confirmed the formation of a well-defined orthorhombic phase at 800 °C, with increasing crystallinity compared to lower temperatures. SEM analysis revealed that increasing the treatment temperature from 400 °C to 800 °C leads to particle growth and morphological evolution in Bi₂WO₆, supporting the structural changes observed in XRD. Additionally, smaller particles at lower temperatures form a more uniform composite with CMC by effectively filling interstitial gaps. The gamma-ray shielding performance was first determined through experimental measurements, and then complementary Phy-X/PSD calculations and GAMOS simulations were performed to extend the analysis across a broader energy range of 122 keV to 1408 MeV. At 1275 keV, the sample synthesized at 800 °C exhibited the highest mass attenuation coefficient of 0.060 cm2/g, the lowest half-value layer of 4.752 cm, and the shortest mean free path of 6.855 cm, indicating a trend of enhanced attenuation compared to samples synthesized at lower temperatures. In contrast, as the synthesis temperature decreases, the probability of photons interacting with electrons increases due to the coexistence of many structures in different phases and morphological irregularities, resulting in improved gamma ray shielding performance at low energies. These quantitative improvements demonstrate that thermally optimized bismuth tungsten oxide samples are promising non-toxic, lead-free candidates for efficient gamma-ray shielding applications.