Sustainable Rubberized RCC Using Locally Sourced Waste Rubber Tire Powder and GGBFS-Based Binder


Öztürk İ. Ş., Sarı F. A., Önal Y., Serin S., Emiroğlu M., Güler H., ...Daha Fazla

Polymers, cilt.18, sa.17, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 18 Sayı: 17
  • Basım Tarihi: 2026
  • Doi Numarası: 10.3390/polym18172046
  • Dergi Adı: Polymers
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, Chemical Abstracts Core, Compendex, INSPEC, Academic Search Ultimate (EBSCO), Engineering Source (EBSCO), Materials Science & Engineering Collection (ProQuest), Technology Collection (ProQuest)
  • Anahtar Kelimeler: waste rubber tire powder (WRTP), roller-compacted concrete, ground granulated blast-furnace slag (GGBFS), sustainable construction materials, mechanical properties, microstructural analysis
  • Uşak Üniversitesi Adresli: Evet

Özet

This study investigates roller-compacted concrete (RCC) in which fine aggregate was replaced with waste rubber tire powder (WRTP) at 0–16% by volume, using a binder containing 40% ground granulated blast-furnace slag (GGBFS). Fresh, mechanical, transport-related, microstructural, and environmental aspects were evaluated. While WRTP reduced workability, density, and ultrasonic pulse velocity (UPV), UPV values remained within the “excellent” classification range. Among the investigated mixtures, 2% WRTP provided the most favorable overall performance, increasing the 28-day compressive strength from 26.6 to 28.2 MPa, the 90-day compressive strength from 31.1 to 37.8 MPa, the flexural strength from 3.33 to 3.47 MPa, and the splitting tensile strength from 1.81 to 2.37 MPa. The 2% WRTP mixture also reduced the secondary capillary absorption coefficient by approximately 32.3%, from 0.00127 to 0.00086 mm/√s. Higher WRTP contents progressively decreased compressive strength and static modulus of elasticity, whereas flexural strength was comparatively less affected. SEM/EDS observations revealed more pronounced interfacial voids and discontinuities at higher WRTP contents, consistent with the observed performance decline. A simplified cradle-to-gate embodied-carbon assessment indicated that the 40% GGBFS binder substitution was the primary contributor to the estimated carbon reduction, with the reference and 2% WRTP mixtures exhibiting approximately 33.4% and 33.1% lower embodied carbon, respectively, than the hypothetical cement-only RCC baseline. In addition, the 2% WRTP mixture incorporated 6.43 kg/m3 of waste tire-derived rubber, providing an additional waste-utilization benefit. Overall, low WRTP incorporation, particularly at 2%, combined with a GGBFS-based binder provided a favorable balance between engineering performance, reduced embodied carbon, and waste utilization under the investigated conditions.