Color Stability and Translucency of Two CAD-CAMRestorative Materials Subjected To Mechanical Polishing,Staining, and Prophylactic Paste Polishing Procedures


YILDIRIM B., Recen D.

Ege Üniversitesi Diş Hekimliği Fakültesi, vol.42, no.1, pp.1-8, 2021 (Peer-Reviewed Journal) identifier

  • Publication Type: Article / Article
  • Volume: 42 Issue: 1
  • Publication Date: 2021
  • Journal Name: Ege Üniversitesi Diş Hekimliği Fakültesi
  • Journal Indexes: TR DİZİN (ULAKBİM)
  • Page Numbers: pp.1-8
  • Uşak University Affiliated: Yes

Abstract

Introduction: The aim of this study is to evaluate the translucency and color change of two computer-aided design and computer aided manufacturing (CAD/CAM) blocks after subjected to mechanic polishing, coffee staining, and prophylactic paste polishing procedures. Methods: 26 specimens (n=13) were obtained from each CAD/CAM block (Cerasmart A2-HT; GC, Initial-LRF, A2-HT: GC). Colorchange values were evaluated after subjected to mechanic polishing, coffee staining, and prophylactic polishing procedures. Datawere analyzed by a Shapiro-Wilk normality test and the translucency and color change values were evaluated statistically withFriedman test. Mann Whitney-U test was used to determine the statistical significance between the Cerasmart and Initial-LRF interms of translucency and color change (α=.05). Results: For baseline measurements and after mechanic polishing measurement, the mean translucency value of the Cerasmartwas significantly higher than Initial-LRF (p<0.05). In Cerasmart and Initial-LRF groups, coffee storage significantly increased thecolor change value, polishing with a prophylactic paste significantly decreased the color change value (p<0.05). Discussion and Conclusion: Cerasmart, showed higher discoloration rate in coffee than Initial-LRF, and the translucency values ofboth Cerasmart and Initial-LRF specimens stored in the coffee solution decreased. Also, polishing with a prophylactic paste can berecommended.